논문번호 | 81 | ||
논문제목(영문) | The Control of Drug Release and Vascular Endothelialization after Hyaluronic Acid-Coated Paclitaxel Multi-Layer Coating Stent Implantation in Porcine Coronary Restenosis Model. | ||
국내외구분 | 국내 | SCI여부 | SCI(E) |
연구책임자역할 | 공저자 | ||
주저자명 | Bae IH | ||
교신저자명 | Jeong MH | ||
공동저자명 | Bae IH, Jeong MH, Kim JH, Park YH, Lim KS, Park DS, Shim JW, Kim JH, Ahn Y, Hong YJ, Sim DS. | ||
게제년월일 | 2016-10-07 | ||
ISSN | 1738-5520 | ||
Impact Factor | 0.706 | ||
학술지명 | Korean circulation journal. | ||
서지사항 | N집 / 47권 / 1호, 페이지(123 - 131) | ||
요약초록문 (Abstract) 입력 |
Abstract BACKGROUND AND OBJECTIVES: Hyaluronic acid (HA) is highly biocompatible with cells and the extracellular matrix. In contrast to degradation products of a synthetic polymer, degradation products of HA do not acidify the local environment. The aim of this study was to fabricate an HA-coated paclitaxel (PTX)-eluting stent via simple ionic interactions and to evaluate its effects in vitro and in vivo. MATERIALS AND METHODS: HA and catechol were conjugated by means of an activation agent, and then the stent was immersed in this solution (resulting in a HA-coated stent). After that, PTX was immobilized on the HA-coated stent (resulting in a hyaluronic acid-coated paclitaxel-eluting stent [H-PTX stent]). Study groups were divided into 4 groups: bare metal stent (BMS), HA, H-PTX, and poly (L-lactide)-coated paclitaxel-eluting stent (P-PTX). Stents were randomly implanted in a porcine coronary artery. After 4 weeks, vessels surrounding the stents were isolated and subjected to various analyses. RESULTS: Smoothness of the surface was maintained after expansion of the stent. In contrast to a previous study on a PTX-eluting stent, in this study, the PTX was effectively released up to 14 days (a half amount of PTX in 4 days). The proliferation of smooth muscle cells was successfully inhibited (by 80.5±12.11% at 7 days of culture as compared to the control) by PTX released from the stent. Animal experiments showed that the H-PTX stent does not induce an obvious inflammatory response. Nevertheless, restenosis was clearly decreased in the H-PTX stent group (9.8±3.25%) compared to the bare-metal stent group (29.7±8.11%). CONCLUSION: A stent was stably coated with PTX via simple ionic interactions with HA. Restenosis was decreased in the H-PTX group. These results suggest that HA, a natural polymer, is suitable for fabrication of drug-eluting stents (without inflammation) as an alternative to a synthetic polymer. |
||
파일 |
B81.The+Control+of+Drug+Release+and+Vascular+Endothelialization+after.pdf (16.9M) DATE : 2021-05-21 11:34:47 |